Smithy No. 4 · Tanners' Wynd · Coal smoke since MDCCLXI

Halla Forge

“Work it hot, quench it true.” — Heat is the only gauge in this shop. Watch the bar; the colour tells you when to swing.

20 °C stock cold
Drawn out0%
Shoe bend0%
Scaling / burn0%
Crack risk0%

Rules of the Fire

Four maxims, Halla & Son
I.

Never trust the pyrometer, trust the eye

A dial is a suggestion. Iron at 800 °C says dark cherry, at 1000 °C plain orange, at 1150 °C yellow like a butter candle. The bar on this bench is coloured by those same numbers — when it reads right, swing.

II.

Strike hot, or strike nothing

Steel below the cherry is not being forged, it is being bullied. Cold blows come back as cracks and a dead sound the whole wynd can hear. A hot blow rings; a cold blow thuds. Halla's grandfather could tell a cold bar by ear alone.

III.

Fire eats coal, bellows eats patience

Pumping air lifts the coal bed several hundred degrees and brings a green bar to cherry in half the time — but it also takes a careless bar to scaling past 1230 °C, where the iron gives off sparks and flakes like burnt pastry. Watch the burn meter or weld a new bar next winter.

IV.

The quench is a promise

Water at the wrong heat is the wrong shoe. Bring a shoe-ready bar to the bucket above hardening heat and the steel takes Halla's mark; quench a cold, straight, lazy bar and the mare will tell you about it by Thursday.

The Smith's Tongue

A working glossary
Drawing out
Shortening the hammer's journey and lengthening the bar's — each blow spreads the iron thinner and longer. Volume is never lost, only persuaded.
Upsetting
The reverse: driving length back into thickness by standing the bar on the anvil and swinging at the sky. Halla's son calls it “folding time in half”.
Scaling
Iron oxide blooming off hot steel above ≈1200 °C — dark flakes, showering sparks, and carbon leaving the party. A little is housekeeping; a lot is a burnt bar.
Weld heat
≈1300 °C, yellow-white, sparks flying like a struck match. The heat at which two faces of iron join — and the heat at which most apprentices lose a bar.
Fuller
A rounded-shouldered tool laid across the bar to spread a dent into a line. Use it where a hammer alone would only make a valley.
Hardy hole
The square socket in the anvil's heel that holds cut-offs, swages and the fuller itself. Nothing fancy; everything hangs off it.
Pritchel
A slender punched-drift for drifting nail holes in the finished shoe — a horseshoe without holes is just a paperweight shaped like one.
The horn
The tapered beak at the anvil's end, made for bending. Rest a hot end over it and every blow curves the bar toward a hoof.
Bench legend Drag the bar — rack ↔ coals ↔ anvil Click anvil or Space — strike Slide right — end over horn = bend B — bellows Sound off until you say otherwise